In-process monitoring and qualification of SLM produced nickel based superalloys using eddy current inspection method and a novel EC array probe design

Is this your thesis?

This record came from a bulk archive import. If it’s yours, link it to your profile.

2022
1 views
1 downloads

Abstract (EN)

Additive manufacturing gives high flexibility to part designers on the manufacturability of optimized and complex parts. This advantage brings a part inspectability challenge. In this study, the Eddy Current Array sensor application is investigated as an in-process monitoring/inspection method and discussed as an L-PBF layer acceptance technique for the volumetric qualification of aerospace parts. Laser Powder Bed Fusion (L-PBF) process produced Inconel 625 test samples are used for data collection. Intentionally defects are created by using a waterjet-guided laser system to trial the L-PBF in-process eddy current inspection capability.

Author

Erdem Bektaş

How to Cite

Erdem Bektaş (Doctorate thesis). In-process monitoring and qualification of SLM produced nickel based superalloys using eddy current inspection method and a novel EC array probe design, 2022, Koç University.

License

Tüm Hakları Saklıdır

This work is shared under the specified license terms.

More theses from Koç University